Waspaloy bụ nickel base age hardable superalloy nwere oke okpomọkụ dị elu yana ezigbo nguzogide corrosion, ọkachasị na oxidation, na okpomọkụ ọrụ ruo 1200°F (650°C) maka ngwa ntụgharị dị egwu, yana ruo 1600°F (870°C) ) maka ngwa ndị ọzọ, obere ihe na-achọsi ike, ngwa.The alloy si elu okpomọkụ ike na-ewepụtara ya siri ike ngwọta ike ọcha, molybdenum, cobalt na chromium, na afọ hardening ọcha, aluminum na titanium.Ike ya na nkwụsi ike ya dị elu karịa nke dị maka alloy 718.
C | S | P | Si | Mn | Ti | Ni | Co | Cr | Fe | Zr | Cu | B | Al | Mo |
0.02 0.10 | ≤ 0.015 | ≤ 0.015 | ≤ 0.15 | ≤ 0.10 | 2.75 3.25 | Bal | 12.0 15.0 | 18.0 21.0 | ≤ 2.0 | 0.02 0.08 | ≤ 0.10 | 0.003 0.01 | 1.2 1.6 | 3.5 5.0 |
Njupụta (g/cm3 ) | 0.296 | |||||
Ebe mgbaze (℃) | 2425-2475 | |||||
Emperature(℃) | 204 | 537 | 648 | 760 | 871 | 982 |
Ọnụọgụ mgbasawanye okpomọkụ | 7.0 | 7.8 | 8.1 | 8.4 | 8.9 | 9.7 |
Thermal conductivity | 7.3 | 10.4 | 11.6 | 12.7 | 13.9 | - |
Modulu nke na-agbanwe agbanwe(MPax 10E3) | 206 | 186 | 179 | 165 | 158 | 144 |
Ọnọdụ | Ike tensile/MPa | Ọnọdụ okpomọkụ na-arụ ọrụ |
Ngwọta annealing | 800-1000 | 550ºC |
Ngwọta+ ịka nká | 1300-1500 | |
Na-ewe iwe | 1300-1600 | |
Mmiri na-ewe iwe | 1300-1500 |
¤(Arụmọrụ dị elu na-adịgide adịgide, nwalee maka mpempe akwụkwọ ọgwụgwọ okpomọkụ)
Ogwe/Ogwe /Waya/ịgha | Eriri / eriri igwe | Mpempe akwụkwọ/efere | |
ASTM B 637, ISO 9723, ISO 9724, SAE AMS 5704, SAE AMS 5706, SAE AMS 5707, SAE AMS 5708, SAE AMS 5709, SAE AMS 5828, | SAE AMS 5544 |
Age hardening pụrụ iche nickel dabeere alloy, elu irè ike na 1400-1600 ° F.Good iguzogide ọxịdashọn eji na gas turbine engine na 1400-1600 ° F ikuku.Na 1150-1150 Celsius F, Waspaloy creep ike mgbawa dị elu karịa na 718.
Na ọnụ ọgụgụ nke 0-1350 ° F, ike tensile na-ekpo ọkụ maka obere oge dị njọ karịa 718 alloy
A na-eji Waspaloy maka akụrụngwa turbine gas nke na-achọ ike dị ukwuu na nguzogide corrosion na okpomọkụ dị elu.fasteners na ndị ọzọ dị iche iche engine ngwaike, airframe mgbakọ na mwepụ ngwa agha.